You should not routinely wet pine between sandpaper grits; water-based "wet sanding" or "water popping" is occasionally useful on pine when you want to raise crushed grain for a smoother final finish, but it risks grain swelling, raised fuzz, stain blotchiness, and uneven color, so it is a technique to use deliberately rather than a default step.

The question mixes two different practices that carpenters sometimes blur together. One is wet sanding, where you sand with water or a lubricant to control dust and keep the abrasive from clogging—common on automotive finishes, cured film finishes, and some metals, but not standard on bare softwood. The other is water popping (also called grain raising or "sponging"), where you deliberately dampen bare wood so that crushed fibers swell, let it dry, then sand the raised fibers back down. That second technique is the one people actually mean when they ask about wetting pine between grits. Pine is a softwood with pronounced earlywood/latewood contrast and a strong tendency to absorb water unevenly, which is why the answer is "sometimes, carefully" rather than "yes" or "never."

What "wetting between grits" is actually for

Bare wood that has been planed or sanded has some fibers bent over and compressed rather than cut cleanly. On a finish that sits on the surface (film finishes like polyurethane, lacquer, shellac, or varnish), those crushed fibers can pop up when the first coat of finish wets the wood, leaving a rougher surface than the sanding suggested. Water popping pre-triggers that swelling on bare wood: you wipe or mist the surface with clean water, the fibers stand up, the wood dries, and you sand the raised fibers off with the next grit. The result is a flatter surface and, on some woods, a more even absorption of stain.

The logic is sound and it works. The problem is that pine is one of the least forgiving woods for this treatment, for reasons explained below.

Why pine is a difficult candidate

Uneven absorption. Pine's earlywood (the lighter, softer bands) is far more porous than its latewood (the darker, denser bands). Water soaks into earlywood quickly and into latewood slowly. A damp wipe therefore swells the two bands by different amounts and at different rates. You can end up with a surface that is not just "raised" but differentially raised—and sanding that back to flat removes more of the soft earlywood than the hard latewood, which can deepen the texture rather than smooth it.

Raised grain that will not sand away cleanly. Water-raised fibers on pine can be frizzy and soft. Sanding them can smear rather than cut them, especially with worn paper or too fine a grit, producing a fuzzy surface that finish will make look worse.

Stain and finish blotchiness. Pine is already notorious for blotchy stain absorption. Adding water changes the moisture content and can redistribute extractives and resins near the surface. If the wood is not fully dry before staining, or if the dampening was uneven, the stain can take unevenly. On pine, this is a real practical risk, not a theoretical one.

Swelling, warping, and joint movement. Water swells wood across the grain. Thin panels, wide glue-ups, and pieces with mixed grain orientation can cup or move. If you are working on an assembled project, moisture can also affect joints and adjacent surfaces.

Drying time and moisture content. You cannot sand or finish until the wood is back near its equilibrium moisture content. In a humid shop, that can take much longer than expected, and "dry to the touch" is not the same as "dry enough to finish."

When it can make sense on pine

There are narrow situations where a light water pop helps:

You are aiming for a very smooth painted finish on a softwood and want to knock down grain fuzz before primer. A light mist, full dry, and a pass with the next grit can reduce the "whiskering" that shows through paint. You are staining a pine piece and want to reduce, not eliminate, blotchiness, and you are already using a wood conditioner or a washcoat. Water popping before conditioning can give a slightly more uniform surface, but it is not a substitute for a conditioner on blotch-prone pine. You are working a small, flat, solid-pine panel where movement is not a concern and you can control drying.

In all of these, the method matters: mist or wipe lightly and evenly, do not soak, let it dry completely (often 12–24 hours in a normal shop, longer in humid conditions), then sand the raised fibers with the next grit—not the same grit you just used, and not a jump to a very fine grit.

When you should not do it

On thin stock, wide panels, or assembled projects where swelling and movement are a risk. When you plan to stain and have not tested on scrap. Pine's blotching is unpredictable; test the exact sequence on an offcut from the same board. When the wood is already at a high moisture content or the shop is humid. Adding water makes drying unpredictable. As a substitute for proper sanding technique. If your surface is rough because you skipped grits or used dull paper, water popping will not fix it. Between every grit. This is the key misconception in the question. Water popping is typically a one-time step, usually after the last "shaping" grit and before the final smoothing grit or before finish. Doing it between each grit multiplies the swelling/drying cycles, increases risk, and wastes time.

The "wet sanding" confusion

Separately, some woodworkers wet-sand cured film finishes with water and fine abrasive to level the finish—this is a finishing technique on the finish, not on bare wood, and it is not what "between sandpaper" usually implies for bare pine. Wet sanding bare pine with water as a lubricant is not a standard or recommended practice: it clogs paper, raises grain, and creates a slurry that can drive dirt and extractives into the pores. If someone tells you to "wet sand pine," clarify whether they mean water popping bare wood, wet-sanding a cured finish, or using a lubricant like mineral spirits (which some use on bare wood to reduce dust and clogging—but that is a solvent, not water, and has its own cautions).

A practical sequence if you choose to water pop pine

1: Sand through your normal grits up to the one just before your final smoothing grit. 2: Mist or wipe the surface evenly with clean water—damp, not soaked. Avoid puddles and avoid letting water sit. 3: Let it dry completely. Judge by moisture, not by clock; a moisture meter helps if you have one. 4: Sand the raised fibers with the next grit, using light pressure and fresh paper. 5: Remove dust thoroughly. 6: If staining, test on scrap first; consider a conditioner or washcoat. 7: Apply finish only when moisture content is back to a normal level for your shop and climate.

The bottom line

Wetting pine between sandpaper grits is not a standard step and is not something to do routinely. It is a targeted technique—water popping—that can help with grain raising and, in some cases, stain uniformity on pine, but pine's uneven absorption, blotchiness, and movement make it riskier than on hardwoods like maple or cherry. If you use it, do it once, lightly, on stable stock, with full drying and a test on scrap. If your goal is just a smooth surface, better sanding discipline and sharp paper will do more than water will.

The main ambiguity in the question is whether "wet" means water popping bare wood or wet sanding with water as a lubricant; the first is occasionally defensible on pine, the second is not standard practice for bare softwood.