A stripped screw hole in plastic is repairable, and the best method depends on the plastic and the load. For most household plastics—ABS, polycarbonate, PVC, and appliance housings—the rotating fix is to enlarge the hole slightly, fill it with a stronger material, and drive the screw into that new material. The quickest version uses a plastic-compatible adhesive plus baking soda or a scrap-plastic plug; the strongest version uses a threaded insert. The key condition is that you match the repair to whether the plastic is a rigid, solvent-bondable thermoplastic or a soft, waxy, or fiber-filled composite that glue won't grip.
First, diagnose why the hole failed
A stripped screw hole isn't one problem. It's a symptom, and the fix has to address the cause or the repair fails the same way.
The most common cause is over-torquing during installation or removal. Plastic threads deform under load far more easily than metal, and once the threads smear, the screw spins without biting. The second cause is repeated disassembly—every insertion and removal wears the threads a little, and appliance covers, laptop bottoms, and electronics cases often see a dozen cycles. The third cause is material fatigue or chemical damage: UV-exposed outdoor plastic, heat-cycled engine-bay plastics, and solvent-wiped surfaces lose strength and crumble at the thread roots. The fourth is a hole that was oversized from the factory or drilled too large by a previous repair.
You can tell which you have with a simple check. Drive the original screw in by hand with a screwdriver, not a drill. If it spins freely with almost no resistance, the threads are gone and the hole needs new material. If it bites but slips under load, the threads are damaged but the hole geometry survives—those are the easiest cases. Shine a light into the hole: white, powdery residue suggests crumbling plastic (common in old or heat-damaged parts), while a clean, smooth bore suggests simple thread wear.
Stop and reconsider if the plastic is visibly cracked radiating from the hole, if the surrounding boss (the raised cylinder around the hole) has split, or if the part is structural—a load-bearing bracket, a safety cover, or anything holding weight. In those cases, a glue-and-screw fix can fail suddenly, and the part needs replacement or a proper mechanical repair by someone qualified to judge the load.
What you need before you start
Gather these before touching the screw:
The original screw, or a replacement of the same diameter, thread pitch, and length. Pan-head sheet-metal or machine screws are common; note whether the screw is self-tapping (coarse threads for plastic) or machine-threaded (fine threads, often into a metal insert). Isopropyl alcohol (90% or higher) and cotton swabs for cleaning. A plastic-compatible adhesive. Cyanoacrylate (CA/super glue) works on many rigid plastics but is brittle; two-part epoxy is stronger and gap-filling; specialty plastic adhesives (often methyl methacrylate or solvent-based) bond specific plastics best. Check the label for the plastic type. Baking soda (sodium bicarbonate) or a scrap of matching plastic, plus a file or sandpaper to make shavings or a plug. A drill bit slightly larger than the current hole, and a drill. Optional but stronger: a threaded insert kit sized to the screw, or a heat-set insert if the plastic is a thermoplastic that tolerates heat. Clamps or tape to hold parts steady, and a small pick or awl to clear debris.
One caution before you buy anything: adhesive compatibility is plastic-specific. Polyethylene and polypropylene (common in buckets, some toys, and flexible containers) are notoriously hard to glue—almost nothing bonds them well without surface treatment—so for those, mechanical fixes like a larger screw or an insert beat adhesive repairs. Check the recycling code molded into the part if you can find it.
Method 1: The baking-soda and cyanoacrylate fill (fastest, good for light loads)
This is the standard bench fix for small electronics and household plastic because it sets in minutes and the baking soda makes the CA glue set harder and less brittle than glue alone.
1: Remove the screw and clean the hole with isopropyl alcohol on a swab. Let it dry fully—CA glue won't bond to a wet or oily surface. 2: If the hole is ragged, ream it lightly with the drill bit by hand or at low speed to create clean walls. Don't enlarge it more than necessary. 3: Pack the hole with baking soda using a small funnel made from paper, or dip a toothpick in glue and then into baking soda to build up layers. Work in thin layers rather than filling the whole hole at once. 4: Apply a drop of CA glue to the baking soda, let it cure, and repeat until the hole is slightly proud of the surface. The mixture hardens within seconds to a minute. 5: File or sand the plug flush, then drill a pilot hole smaller than the screw's minor diameter. 6: Drive the screw in by hand, stopping when it seats. Don't over-torque.
The success check: the screw should resist turning with moderate hand pressure and hold when you gently tug the part. If it spins, the plug didn't bond to the walls—clean and repeat, or move to a stronger method.
This method works best on rigid, smooth plastics like ABS and polycarbonate. It's a poor choice for flexible plastics, because the plug is rigid and will crack away from a bending surface.
Method 2: The scrap-plastic plug (best on solvent-bondable thermoplastics)
If you can identify the plastic and it's a solvent-bondable thermoplastic—ABS, styrene, acrylic, polycarbonate, PVC—you can often weld in new material that behaves like the original.
1: Clean the hole as above. 2: Make plastic shavings or a small plug from a scrap of the same plastic. Shavings from a hidden interior surface are ideal because color and composition match. 3: Pack the shavings into the hole and add a few drops of solvent cement (the same type used for plastic plumbing or model building, matched to the plastic). For ABS, acetone or ABS cement works; for acrylic, a acrylic solvent cement; for PVC, PVC pipe cement. 4: Let it set per the cement's instructions—usually several hours for full strength. 5: Drill a fresh pilot hole and drive the screw.
The advantage here is a genuinely homogeneous repair: the new material fuses to the old, so the thread grips like original plastic. The limitation is that you must know the plastic type, and solvent cements are strong-smelling and flammable, so work with ventilation and away from ignition sources.
Method 3: The threaded insert (strongest, for parts that come apart repeatedly)
When a screw hole will be used again and again—laptop hinges, equipment panels, 3D-printed parts, appliance housings—no adhesive plug survives repeated cycling. A threaded insert is the durable answer.
Two insert types matter. Heat-set inserts are brass and are pressed into a slightly undersized hole with a soldering iron; the heat melts the surrounding thermoplastic, and the insert locks in as it cools. They require a thermoplastic that softens without burning—PLA, ABS, PETG, and most common 3D-printing filaments qualify, but thermosets and some composites don't. Threaded inserts for plastic also come in press-fit and self-tapping versions that cut their own threads into a drilled hole.
The procedure for a heat-set insert:
1: Measure the insert's outer diameter and choose a drill bit that matches the insert manufacturer's recommended hole size—typically slightly smaller than the insert's widest point so the plastic grips it. 2: Drill the hole to the correct depth, slightly deeper than the insert is long. 3: Thread the insert onto the tip of a soldering iron held at a moderate temperature (start around 200–230°C / 390–445°F and adjust—too hot scorches the plastic). 4: Press the insert straight into the hole until its top is flush with the surface. Keep it vertical; tilting ruins the alignment. 5: Let it cool completely before driving the screw.
The success check: the insert shouldn't spin when you turn a screw into it, and it should sit flush and perpendicular. If it spins, the hole was too large—remove it and use a larger insert or fall back to an epoxy-set insert.
Epoxy-set inserts work on plastics that can't take heat: drill the hole, coat the insert's exterior with two-part epoxy, seat it, and let it cure fully before use. This is slower but works on nearly any rigid plastic.
Method 4: The larger screw or the through-bolt (simple mechanical fallback)
Sometimes the simplest fix is to change the fastener. A screw one size larger in diameter will cut new threads into the existing hole, provided the surrounding boss is thick enough to take it. Go up one size at a time, and check that the screw head still fits its countersink or recess.
If the boss is thin or cracked, a through-bolt with a nut and washer on the back side is stronger than any thread repair—but only if you can access the back. This is common on enclosures, brackets, and furniture where the reverse side is open. Use a washer under the nut to spread load, and don't overtighten; plastic compresses.
When none of these fit—cracked boss, inaccessible back, structural part—the honest answer is replacement. A repair that fails under load is worse than a part swap, especially on anything holding weight, sealing a fluid, or protecting a user.
Matching the repair to the plastic
The single biggest predictor of a lasting repair is plastic type, and it's worth a minute to identify it. Look for the recycling code or a material stamp. Here's how the methods sort out:
| Plastic type | Common examples | Best method | Avoid |
|---|---|---|---|
| ABS | Electronics housings, toys, appliance covers | Baking soda + CA, solvent plug, heat-set insert | Nothing major; very repairable |
| Polycarbonate | Clear guards, tool housings | Baking soda + CA, solvent plug | Aggressive solvents that craze it |
| PVC | Pipe fittings, outdoor trim | Solvent cement plug, insert | CA alone (brittle) |
| Acrylic | Displays, guards | Solvent cement plug | Heat (melts and blisters) |
| Polyethylene / polypropylene | Buckets, flexible containers, some toys | Larger screw, through-bolt, mechanical only | Most adhesives (poor bond) |
| Nylon | Gears, bushings, some tools | Epoxy, insert | Solvents (resistant) |
| Fiberglass/composite | Panels, boats, some housings | Epoxy + insert, mechanical | Solvent welding |
Two edge cases deserve a note. First, glass-filled or fiber-reinforced plastics drill and tap poorly and glue unpredictably—threaded inserts set in epoxy are usually the only reliable route. Second, foamed or honeycomb-core plastics have almost no material around the hole; a repair plug has nothing to anchor to, so you need to back the hole with a plate or use a through-fastener.
Why repairs fail, and how to prevent it
Most failed repairs fail for one of four reasons, and each is preventable.
The surface wasn't clean. Mold release agents, oils, and dust are on nearly every molded part. Wipe with isopropyl alcohol and let it dry; for stubborn contamination, lightly abrade with fine sandpaper first.
The plug didn't bond to the walls. Filling a hole and drilling into the plug only works if the plug is anchored. Underfill or a contaminated bore leaves a plug that spins free. Pack firmly against the walls, and let adhesives cure fully—CA is fast, but epoxy needs its full rated time, often 24 hours, for strength.
The screw was over-torqued. Plastic threads strip at far lower torque than metal. Drive by hand and stop at snug; a clutch-adjusted drill driver on its lowest setting is acceptable for assembly but risky for repair. If you must use power, test the clutch on a scrap first.
The repair was undersized for the load. A baking-soda plug holds a cover panel fine; it won't hold a hinge under repeated stress. Match the method to the load, and when in doubt, overbuild with an insert.
A useful preventive habit for parts you'll disassemble again: apply a tiny amount of thread lubricant (a wax or a plastic-safe grease) to the screw, and never exceed the original torque. Lubricated threads wear the plastic less on each cycle, which is exactly what strips holes over time.
A worked example: fixing a stripped laptop-bottom screw
Say a laptop's bottom cover has one stripped screw hole, and the cover rattles. The plastic is almost certainly ABS or a PC/ABS blend. You have no insert kit and want a same-day fix.
Clean the hole with alcohol, pack it with baking soda, and wick in thin CA glue in two or three layers until the hole is filled proud. Let it cure, file flush, and drill a pilot hole about 80% of the screw's minor diameter—if the screw's core is roughly 2 mm, drill about 1.6 mm. Drive the original screw by hand until it seats. Expect the repair to hold for normal use; if the cover comes off monthly, plan to install a heat-set insert next time, because the CA plug will eventually fail under repeated cycling.
The check that matters: after assembly, gently press and lift the corner of the cover. If it moves independently of the screw, the plug didn't anchor—disassemble and redo with more packing or epoxy. If it's solid, you're done.
When the hole can't be saved
Some failures are beyond a bench repair, and recognizing them saves time and prevents a worse outcome. A boss that has split down its length, a hole that sits at the edge of a thin panel with no material around it, or a part that carries a load or seals a fluid all call for replacement rather than patching. On safety-relevant parts—ladders, load-bearing brackets, pressure housings, vehicle structural components—don't improvise. A failed repair there can hurt someone. Have the part replaced or evaluated by someone qualified for that application.
For ordinary household, electronics, and hobby plastic, though, the methods above cover nearly every case. The pattern is consistent: clean the hole, replace the lost material with something stronger, and drive the screw gently into the new material. The only real decisions are which plastic you have and how much load the joint must carry—and both point clearly to one method.